Got a job coming up in a couple weeks. I'm installing gradus ejc50 constructin joint cover. Normally I'd use f60 but the area is sensitive so a solvent based product is out of the question. Not sure weather to use f66 or uzin wk222 not really familiar with either product or is there something better out there. It will be getting fitted between polyflor xl and welded along both edges.
Thanks for the advice guys ill give the uzin a try. The area is occupied so is warmshouldn't take too long to go off.
Prob with the uzin one it takes ages to go off. We got a tub in after seeing a demo of it but we only used it once. Most showers we do only have 2 walls to cove up so want to be in and out. Be better used on a big job were you have time to wait