Using a gypsum smoothing compound still needs a primer onto the anhydrite screed and the gypsum can take a few days to dry. We use a penetrating...
Unfortunately these types of screeds are here to stay, we have always double primed before applying the smoothing compounds and never had a...
I would ask the builder for a data sheet on the Cemfloor as the preferred screed with underfloor heating tends to be anhydrite due to the flow...
Hi Mani and happy New year to you. Is the subfloor in the kitchen concrete? Making a floor level is going to be expensive and do you have the...
Ensure the floorboards are secure, any bad dips to the boards use a latex underlayment ie sx300na to fill and then overlay with 6mm marine grade...
What floorcovering are you installing?
We would.normally use sx300na if the floor boards are bad before overlaying with plywood and if using an acrylic adhesive we would prime the plywood.
You can use a latex screed to pack the dips then overlay with min 6mm wbp plywood screw fixed 100/150mm centres with ring nails. Depending on the...
The comment someone made above about getting the underfloor heating on is a good start, make sure you commission the heating as per the...
Very true, getting correct information from the builder can be difficult.
200Sqm is a decent size area, ring the manufacturer of smoothing compound technical department the number will be on the bag and drums and ask for...