    How come?
     
  2. tarkett85

    tarkett85 Well-Known Member

    3,183
    484
    83
    they don't go very far for what you pay and take much longer to dry than 1k turbo, also when you open a tub you can't re-seal and use the leftovers another day.
     
  3. dazlight

    dazlight Super Moderator

    7,206
    1,704
    113
    Laybond rapid dpm does the same job as 1k as used both of them. I feel saver using a epoxy dpm as with most of them it leaves a thicker coat of dpm on.
     
  4. Matt

    Matt Well-Known Member Staff Member

    6,328
    1,402
    113
    Epoxy DPM = creates a barrier on top of subfloor

    1K turbo (laybond? not sure as not used) = turns the top surface of subfloor into DPM.

    Out of the two i 'personally' prefer 1K turbo. Reasons as above.